Staining in glazes ranges from honey yellow to dark brown, at addition from 1-8%. Impured iron oxide, therefore very affordable.
Fe2O3 - Molar weight: 160
Chem. analysis in %:
Fe2O3 90-96; SiO2/Al2O3 4.00; Loss of ignition 1000°C 1.0.
Grinding fineness in %:
> 45 µm 0.10; primary particle size 0.2 µm.