Application:
Anthrazite coloured stoneware body for handbuildung and for modelling works. Very nice if glazed partially and the unglazed body is in contrast to the glazed parts.
Application temperature: 1000 - 1300°C
Specifications:
Grog / Graining: 25% / 0-0.5mm
Drying shrinkage: 5.3%
1100°C: 2.7% Firing shrinkage / 8.5% Water absorption
1200°C: 4.3% Firing shrinkage / 4.6% Water absorption
1300°C: 5.3% Firing shrinkage / 1.7% Water absorption
Sintering (WA ≤2%) 1260°C approx.
TEC (20-400°C) 62 * 10-7/K (Pre-firing: 1200°C)